The injection screw is the core component of the injection molding machine, and the screw is operated under high temperature, high pressure, high mechanical torque and high friction environment for a long time, and the wear problem is inevitable. Generally, the screw has been surface nitrided to increase the surface hardness, that is, Improve anti-wear ability.

However, if the cause of wear is neglected, and the wear is not reduced as much as possible, the working life of the screw will be greatly reduced.
The granular plastic enters the barrel from the hopper, and it will first reach the feed section. Dry friction will inevitably occur in the feed section. When these plastics are insufficiently heated and unevenly melted, it is easy to cause increased wear on the inner wall of the barrel and the surface of the screw.
Similarly, in the compression section and the homogenization section, if the melting state of the plastic is disordered, it will also cause increased wear.
In the injection of these plastics, if the high speed is used, the shear force on the plastic will be increased, and the reinforcement will produce correspondingly more shredded fibers. The shredded fibers contain sharp ends, which cause wear The force is greatly increased. When inorganic minerals glide on the metal surface at high speed, its scraping effect is not small. Therefore, the speed should not be adjusted too high.